Filter:
 
Material
 
Datasheet pdf available.
Datasheet pdf not available.
 
Standard types according to DIN EN 61212.
 
Tubes made from industrial laminated materials.
 
Value: Minimum requirements of DIN EN 61212.
Value: Typical values, general recommended values, which must not be used as standard values.
 
(1): The flexural strength measured at 150 °C ± 3K must not be less than 50% of the defined value.
(2): After 96 h pretreatment in air at 105 °C ± 5K directly prior to testing and immediate immersion in the hot oil.
 
MaterialCharacteristic property applicationsResinSubstrate
AS EP GC 21Electrical and mechanical applications, TC 130EpoxyWoven glass cloth
AS EP GC 22As type 21 but with TC 155EpoxyWoven glass cloth
AS EP GC 23As type 21 but with combustibility according to UL 94 V-0EpoxyWoven glass cloth
AS EP MP 21Epoxy mica paper, electrical applications at high temperaturesEpoxyMica paper
AS MF GC 21Resistant to arcs and trackingMelamineWoven glass cloth
AS PF CC 21Mechanical and electrical applications, fine weavePhenolicWoven cotton cloth
AS PF CC 22Mechanical and electrical applications, coarse weavePhenolicWoven cotton cloth
AS PF CC 23Mechanical applications, very coarse weavePhenolicWoven cotton cloth
AS PF CC 24Mechanical and electrical applications, very fine weavePhenolicWoven cotton cloth
AS PF CP 21Electrical and mechanical applications at low voltagesPhenolicCellulose paper
AS PF CP 22Electrical applications at high-voltage mains frequencyPhenolicCellulose paper
AS PF CP 23As type 21 but with better electrical propertiesPhenolicCellulose paper
AS PF GC 21Very high mechanical strength at moderate temperaturesPhenolicWoven glass cloth
Availability
 
Datasheet pdf available.
Datasheet pdf not available.
 
Standard types according to DIN EN 61212.
 
Tubes made from industrial laminated materials.
 
Value: Minimum requirements of DIN EN 61212.
Value: Typical values, general recommended values, which must not be used as standard values.
 
(1): The flexural strength measured at 150 °C ± 3K must not be less than 50% of the defined value.
(2): After 96 h pretreatment in air at 105 °C ± 5K directly prior to testing and immediate immersion in the hot oil.
 
AvailabilityDiameter
Unitmm
AS EP GC 212-250
AS EP GC 222-250
AS EP GC 232-250
AS EP MP 212-250
AS MF GC 212-250
AS PF CC 212-250
AS PF CC 222-250
AS PF CC 232-250
AS PF CC 242-250
AS PF CP 212-250
AS PF CP 222-250
AS PF CP 232-250
AS PF GC 212-250
Physical Properties
 
Datasheet pdf available.
Datasheet pdf not available.
 
Standard types according to DIN EN 61212.
 
Tubes made from industrial laminated materials.
 
Value: Minimum requirements of DIN EN 61212.
Value: Typical values, general recommended values, which must not be used as standard values.
 
(1): The flexural strength measured at 150 °C ± 3K must not be less than 50% of the defined value.
(2): After 96 h pretreatment in air at 105 °C ± 5K directly prior to testing and immediate immersion in the hot oil.
 
Physical PropertiesWater absorptionDensityCombustibility
DIN EN 61212-27.27.3UL 94
Test StandardISO 62ISO 1183
Unitmg/cm²g/cm³Category
Min/MaxMax
AS EP GC 211.51.7-1.9-
AS EP GC 221.51.7-1.9-
AS EP GC 231.51.7-1.9V-0
AS EP MP 2121.5-1.8-
AS MF GC 2151.7-1.9V-0
AS PF CC 2151.15-1.35-
AS PF CC 22101.15-1.35-
AS PF CC 23131.15-1.35-
AS PF CC 2451.15-1.35-
AS PF CP 21-1.1-1.2-
AS PF CP 22-1.05-1.15-
AS PF CP 23-1.1-1.2-
AS PF GC 21-1.7-1.9-
Mechanical Properties
 
Datasheet pdf available.
Datasheet pdf not available.
 
Standard types according to DIN EN 61212.
 
Tubes made from industrial laminated materials.
 
Value: Minimum requirements of DIN EN 61212.
Value: Typical values, general recommended values, which must not be used as standard values.
 
(1): The flexural strength measured at 150 °C ± 3K must not be less than 50% of the defined value.
(2): After 96 h pretreatment in air at 105 °C ± 5K directly prior to testing and immediate immersion in the hot oil.
 
Mechanical PropertiesFlexural strength perpendicular to laminationsCompressive strength axialCohesion between layers
DIN EN 61212-25.15.25.3
Test StandardISO 178ISO 604IEC 61212-2
UnitMPaMPaMPa
Min/MaxMinMinMin
AS EP GC 21300175200
AS EP GC 22300 ⁽¹⁾175200
AS EP GC 23300175200
AS EP MP 211006030
AS MF GC 2112080150
AS PF CC 219011090
AS PF CC 228010090
AS PF CC 238010090
AS PF CC 24100120100
AS PF CP 2110010070
AS PF CP 221008070
AS PF CP 2310010070
AS PF GC 21140120200
Electrical Properties
 
Datasheet pdf available.
Datasheet pdf not available.
 
Standard types according to DIN EN 61212.
 
Tubes made from industrial laminated materials.
 
Value: Minimum requirements of DIN EN 61212.
Value: Typical values, general recommended values, which must not be used as standard values.
 
(1): The flexural strength measured at 150 °C ± 3K must not be less than 50% of the defined value.
(2): After 96 h pretreatment in air at 105 °C ± 5K directly prior to testing and immediate immersion in the hot oil.
 
Electrical PropertiesDielectric strength perpendic at 90 ºC in oil (thickness 3 mm)Dielectric strength parallel at 90 ºC in oilInsulation resistancePermittivity 50 HzPermittivity 1 MHzDissipation factor 50 HzDissipation factor 1 MHz
DIN EN 61212-26.16.16.26.36.36.36.3
Test StandardIEC 60243-1IEC 60243-1IEC 60167IEC 60250IEC 60250IEC 60250IEC 60250
UnitkV/mmkVMΩ
Min/MaxMinMinMinMaxMaxMaxMax
AS EP GC 217.7401.000-5.20.50.4
AS EP GC 227.7401.000-5.20.50.4
AS EP GC 237.7401.000-5.20.50.4
AS EP MP 211130100-5.2-0.4
AS MF GC 213.3100.1-8-0.2
AS PF CC 211.61010----
AS PF CC 221.6102----
AS PF CC 231.680.5----
AS PF CC 241.6102----
AS PF CP 21-151----
AS PF CP 229.950 ⁽²⁾1----
AS PF CP 236.1255----
AS PF GC 214.81520---0.4
Thermal Properties
 
Datasheet pdf available.
Datasheet pdf not available.
 
Standard types according to DIN EN 61212.
 
Tubes made from industrial laminated materials.
 
Value: Minimum requirements of DIN EN 61212.
Value: Typical values, general recommended values, which must not be used as standard values.
 
(1): The flexural strength measured at 150 °C ± 3K must not be less than 50% of the defined value.
(2): After 96 h pretreatment in air at 105 °C ± 5K directly prior to testing and immediate immersion in the hot oil.
 
Thermal PropertiesThermal endurance
DIN EN 61212-27.1
Test StandardIEC 60216
UnitT.I.
Min/MaxMin
AS EP GC 21130
AS EP GC 22155
AS EP GC 23130
AS EP MP 21155
AS MF GC 21130
AS PF CC 21120
AS PF CC 22120
AS PF CC 23120
AS PF CC 24120
AS PF CP 21120
AS PF CP 22120
AS PF CP 23120
AS PF GC 21130
 

The above values are provided for general purposes only and not meant to be a specific recommendation for any individual application. All values were determined under laboratory conditions. ASEC Kunststoffen B.V. is not directly neither indirectly responsible for any claim resulting from the use of any information provided in above values. ASEC Kunststoffen B.V. 2016 ©.